High quality astm b265 gr7 titanium foils belt
titanium foil of Product Description
The production process of titanium foil is composed of main working procedure including hot rolling, cold rolling and auxiliary working procedure (pickling, degrease, heat treatment and shearing). Cold rolled titanium strip is the original billet in the process of rolling titanium foil. After pickling and annealing, cold rolled the titanium strip repeatedly and the total amount of deformation is always controlled in 20%~40%. The advanced equipment, rolling process, process control, annealing temperature and time control ensured the surface smoothness and finish of titanium foil, effectively improved the quality of our products.
titanium foil of Procuct Detail
aterial |
CP titanium, titanium alloy |
Grade |
Gr1, Gr2, Gr4, Gr5, Gr7, Gr9, Gr11, Gr12, Gr16, Gr23 etc |
Specification |
Thickness: 0.01~0.1mm, Width: 30~300mm, Length: in coils |
Standard |
ASTM B265, ASTM F67, ASTM F136 etc |
Status |
Hot Rolled(R) Cold Rolled(Y) Annealed(M)Solution treatment(ST) |
Application |
Used in the production of loudspeaker voice diaphragm, filler inside the chemical equipment, medical implants, production of precision parts, etc. |
Titanium foil of show
Titanium foil specifications tolerance range:
Thickness mm |
Tolerance mm |
Width mm |
Tolerance mm |
Length mm |
Tolerance mm |
0.01 ~ 0.02 |
0.003 |
30 ~ 100 50 ~ 300 |
±0.5
|
500min |
0 ~ + 10 |
0.03 ~0.05 |
± 0.005 |
||||
0.06 ~ 0.07 |
± 0.007 |
||||
0.08 ~ 0.09 |
± 0.01 |
||||
0.10 ~ 0.15 |
± 0.015 |
||||
0.18 ~ 0.20 |
± 0.02 |
||||
0.25 ~ 0.30 |
± 0.03 |
||||
0.4 ~ 0.5 |
± 0.05 |
50 ~ 500 |
± 1.0 |
1000min |
0 ~ + 15 |
0.6 ~ 0.9 |
± 0.07 |
2000 (min) |
Grade |
Tensile Strength (min) |
Yield strength 0.2%Offset |
Elongation in 2in.Or 50mm % (min) |
||
Min |
|||||
Ksi |
Mpa |
Ksi |
Mpa |
||
Gr1 |
35 |
240 |
20 |
138 |
20 |
Gr2 |
50 |
345 |
40 |
275 |
18 |
Gr3 |
65 |
450 |
55 |
380 |
18 |
Gr5 |
130 |
895 |
120 |
828 |
10 |
Gr7 |
50 |
345 |
40 |
275 |
18 |
Gr12 |
70 |
483 |
50 |
345 |
18 |